MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BC 304 H3.0 000000 Nylon 6 (PA6), Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: PA 6, injection molding grade, non-reinforced, elastomer-modified, extremely high notched impact strength, including in the dry state and at low temperatures, also applicable for barrier layers in extrusion blow molded containers for e.g. agrochemicals

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.06 g/cc0.0383 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.2 %2.2 %50% RH; ISO 62
Water Absorption at Saturation 7.5 %7.5 %ISO 62
Linear Mold Shrinkage, Flow 0.0114 cm/cm0.0114 in/in150x105x3; 260 °C / MT 80 °C; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0145 cm/cm0.0145 in/in150x105x3; 260 °C / MT 80 °C; 500 bar; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 35.0 MPa5080 psiISO 2093-1
Tensile Strength, Yield 35.0 MPa5080 psi50 mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %50 mm/min, Nominal; ISO 527-1,-2
Elongation at Yield 30 %30 %50 mm/min; ISO 527-1,-2
Tensile Modulus 0.800 GPa116 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 30.0 MPa4350 psi2 mm/min; ISO 178-A
Flexural Yield Strength 25.0 MPa
@Strain 3.5 %
3630 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 0.700 GPa102 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 9.0 %9.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)  17.0 kJ/m²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
 100 kJ/m²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179-1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
Puncture Energy 125 J
@Temperature 23.0 °C
92.2 ft-lb
@Temperature 73.4 °F
ISO 6603-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  3.5
@Frequency 1e+6 Hz
3.5
@Frequency 1e+6 Hz
IEC 60250
 11
@Frequency 100 Hz
11
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm
@Thickness 1.00 mm
889 kV/in
@Thickness 0.0394 in
IEC 60243-1
Dissipation Factor  0.090
@Frequency 1e+6 Hz
0.090
@Frequency 1e+6 Hz
IEC 60250
 0.175
@Frequency 100 Hz
0.175
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °F10°C/min (Dry); ISO 11357-1,-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 270 °C518 °Finjection molding
 260 - 280 °C500 - 536 °F
Mold Temperature 80.0 °C176 °Finjection molding
 80.0 - 90.0 °C176 - 194 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANW9289 / 208094

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.