MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChenGuang 1153 Silicone Resin
Categories: Polymer; Thermoset; Silicone

Material Notes: Properties:
  • Silicone resin are mixtures of solvent (toluene or xylene) with combined hydrolyzates of methyl chlorosilanes and phenyl chlorosilanes contain some amount of hydroxyl groups. The hydroxyl can further condensed into a hard film under heating. Solid content is 50~70% on sale.
  • Outstanding insulation property, high-and-low-temperature resistance, corona and electric arc
  • resistance, water-proof. Outstanding resistance to weather-aging, ozone and chemicals.
  • With silicone resin, the H-grade motor, other electric appliances would be size-small, weight-light, last-long and could be used under harsh environment.
  • When over loaded, the motor or other electric appliance would not go out of order and would not burn heavily. The gasses giving off are not poisonous. The remains after burning is silicon dioxide.
Main Applications: Soft mica-sheet, soft mica-belt, soft glass fabric, glass fabric tube, moisture-proof condenser, dipping and paper treatment

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content >= 50 %
@Temperature 180 °C,
Time 86400 sec
>= 50 %
@Temperature 356 °F,
Time 24.0 hour
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+11 ohm-cm
@Temperature 200 °C
>= 1.00e+11 ohm-cm
@Temperature 392 °F
 >= 1.00e+13 ohm-cm
@Temperature 15.0 - 25.0 °C
>= 1.00e+13 ohm-cm
@Temperature 59.0 - 77.0 °F
 >= 1.00e+12 ohm-cm
@Temperature 15.0 - 25.0 °C,
Time 14400 sec
>= 1.00e+12 ohm-cm
@Temperature 59.0 - 77.0 °F,
Time 4.00 hour
95% moisture
Dielectric Strength  >= 25.0 kV/mm
@Temperature 200 °C
>= 635 kV/in
@Temperature 392 °F
 >= 55.0 kV/mm
@Temperature 15.0 - 25.0 °C
>= 1400 kV/in
@Temperature 59.0 - 77.0 °F
 
Processing PropertiesMetricEnglishComments
Dry Time <= 1.00 hour
@Temperature 200 °C
<= 1.00 hour
@Temperature 392 °F
no copper
Shelf Life >= 6.00 Month>= 6.00 Month
 
Descriptive Properties
AppearanceLight-yellow to golden transparent liquid
Heat Resistance>300hr200°C on copper sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU074 / 255673

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.