- Formulated for electronic, electrical, industrial, artisan, and aerospace applications, including:
- Printed Circuit Boards (PCBs)
- Wire, Cable, and Terminal Lead Tinning and Soldering
- Flat and Round Wire Fabrication
- Semiconductor and Component Lead Tinning
- Stained Glass
- Used for Copper, Beryllium-Copper, Nickel, Alloy 42, Alloy 51, Brass, and some steels.
- VOC-Free formulation is non-hazardous and environmentally friendly.
- Conforms to IPC ANSI J-STD-004, Type ORM1.
- Broad activity range an excellent choice for Tin/Lead, Tin/Silver, Tin/Bismuth, and Indium solder alloys.
Description: Superior Supersafe® No. 30DS contains an amino acid-halide activator which starts to clean metals at room temperature, reaching peak fluxing activity at 260°C/500°F, where it promotes excellent solderability. The broad range of activity makes Superior Supersafe® No. 30DS an ideal choice for high production rates or difficult metal surface conditions where an active, but safe, flux is required.Information provided by Superior Flux
|