MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP29LPSPAO Two Component, Thermally Conductive Epoxy Adhesive
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced; Epoxy, Thermally Conductive

Material Notes: Master Bond Polymer System EP29LPSPAO is a two component, thermally conductive, electrically insulative, high performance epoxy system. It is specially formulated for cryogenic applications and requires a relatively low temperature heat cure. EP29LPSPAO is serviceable at temperatures as low as 4K as an adhesive, sealant, coating and encapsulant, but more importantly, it is able to withstand cryogenic shocks (i.e. room temperature down to liquid helium temperatures in a 5-10 minute time period).

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 4000 - 15000 cPMixed
 2500 - 18000 cPPart B
 55000 - 70000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 75
Tensile Strength >= 5200 psi
Tensile Modulus >= 450000 psi
Shear Strength >= 1000 psiAl/Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cm
Dielectric Constant 4.35
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 - 27.0 µm/m-°C
Thermal Conductivity 9.00 - 10.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 275 °F
Minimum Service Temperature, Air -452 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 5.00 hour
@Temperature 93.3 °C
 5.00 - 7.00 hour
@Temperature 79.4 °C
 8.00 - 10.0 hour
@Temperature 54.4 - 65.6 °C
Pot Life 300 - 420 min100 gram mass
Shelf Life 6.00 Month
@Temperature 23.9 °C
in original unopened containers
 6.00 Month
@Temperature 60.0 °C
in premixed an frozen format
 
Descriptive Properties
Mixing Ratio (A to B)100:65

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP29LPSPAO-1 Black Two Component Epoxy
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy
Master Bond EP37-3FLF Low Exotherm Highly Flexible Two Component Epoxy
Master Bond EP29LPHE Two part, very low viscosity epoxy for bonding, sealing, coating and potting
Master Bond EP29LPAO Two Component Epoxy

PMASTB242 / 132839

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.