MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Michelman® Michem ® NatureShield® 30 Organic Emulsion
Categories: Fluid

Material Notes: NatureShield® products from Michelman are environmentally friendly emulsions and natural oil blends designed to improve the weatherability of exterior surface coatings by providing water resistance and good water bead to wood and concrete. They enhance the natural pattern of wood and can serve as an effective additive in improving the durability and aesthetics of stone based substrates. Usage: Containing 99.5% natural ingredients, this additive imparts good water bead to wood and concrete coatings.

Applications (properties imparted): Concrete (water beading, water resistance), Exterior Wood Protection (water beading, water resistance).

Information provided by Michelman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 29.5 - 30.5 %Non-Volatiles
pH 8.0 - 9.0
Brookfield Viscosity <= 200 cPSpindle #2. 60 RPM.
 
Descriptive Properties
AppearanceOff-white liquid
Emulsifier ChargeAnionic
Recommended pH> 7.0
Solids TypeOrganic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WMICHE9813 / 287408

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.