MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Syncure™ System S117FH Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Typical Properties measured on 20 AWG with 16 mil wall. STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.18 g/ccASTM D792
Deformation 18 %
@Temperature 131 °C,
Time 3600 sec
500 g; UL 1581
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5710 sec; ASTM D2240
 62ASTM D2240
Tensile Strength, Yield 16.5 MPaType IV, 510 mm/min; ASTM D638
Elongation at Break 400 %Type IV, 510 mm/min; ASTM D638
 
Descriptive Properties
AppearanceNatural Color
Automotive SpecificationsSAE J1128
Catalyst Masterbatch40%V-0064G RoHS
Flame TestPassSAE J1128; 45 degree
FormsPellets
Gel Content60%ASTM D2765; Crosslinked PE, Method B (NonReferee Test)
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Grafted Base Resin60%S-1075A
Processing MethodExtrusion Coating
Regional AvailabilityNorth America
Retention of Tensile Elongation120%155°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength100%155°C, 1.91 mm; 168 hr, UL Standard
UsesAutomotive Applications
 Wire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LE0592S Polyethylene
Borealis HE1878E-C2 High Molecular Weight Polyethylene, Crosslinkable
Borealis BorPEX™ HE2557 Yellow High Density Polyethylene Compound for Crosslinked Pipes (Pex-A (Peroxide))
Borealis Borlink™ LH4201R Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE4244R Polyethylene Insulation Compound, Crosslinkable

PH0POL0385 / 144954

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.