A soft and flexible resin produced in a slow drying ester and designed for printing inks and covercoats on ceramic and glass transfers. The product is compatible with common drying and non-drying long oil alkyds. It is compatible with phthalate, sebacate, and maleate plasticisers. Application: Recommended for use in silk screen printing inks and media for the ceramic industry. Information provided by Lucite International |