MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Betaseal™ 1590 CT Polyurethane Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoplastic; Polyurethane, TP

Material Notes: One component, moisture curing adhesive with excellent sag and bead stability based on polyurethane chemistry.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.27 g/cc0.0459 lb/in³
 1.31 g/cc0.0473 lb/in³
Solids Content 98 %98 %
Viscosity Measurement 17 - 23
@Temperature 23.0 °C
17 - 23
@Temperature 73.4 °F
g/min; Ballan, 4mm / 4bar
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 7060 - 70DIN 53505
Adhesive Bond Strength 0.700 MPa
@Time 259000 sec
102 psi
@Time 72.0 hour
Lap shear strength; DIN EN 1465
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 5.00 - 25.0 °C
6.00 Month
@Temperature 41.0 - 77.0 °F
Shelf life is assured at +5°C to +25°C in unopened containers. Short time: 0°C to +40°C
 
Descriptive Properties
ColorBlack
Delivery formCartridges
 Sausages

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDTF9145 / 254238

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.