MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Elkem (Bluestar Silicones) SILCOLAPSE® 411 Silicone Antifoam Compound
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: SILCOLAPSE® 411 is a silicone antifoam compound designed to treat aqueous or non-aqueous media in a wide variety of industries. Its low viscosity and effectiveness in alkaline conditions are of particular interest in a number of applications. SILCOLAPSE® 411 is intended for industrial use only and should not be used in the manufacturing or processing of food, cosmetics or pharmaceuticals

Applications:

  • Chemicals - distillation, extraction, evaporation and filtration processes
  • Oil & Gas - alkanolamine washing of natural or refinery gases.
  • Metallurgy - additive for soluble oils
  • Household Maintenance – manufacturing of waxes and polishes
  • Public works - Asphalt packaging and transportation
Features:
  • Highly effective antifoam in aqueous and non-aqueous processes
  • Effective at low doses, between 1 and 100 ppm
  • Effective over a wide pH range, including alkaline conditions
  • Easy to use, either as is or pre-diluted in a solvent or some of the medium to be defoamed
  • Low viscosity enables use with automatic injection systems.
  • Chemically inert to the media being de-foamed, will not adversely affect processing properties.

Information provided by Bluestar Silicones

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.00 g/cc
Storage Temperature -20.0 - 50.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Descriptive Properties
Appearancegrayish white opalescent liquid
Content100% Active
Diluentsaromatic, aliphatic or chlorinated hydrocarbons, water-soluble solvents

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silberline Sparkle Silvet® 790-30-E1
Silberline Silcroma® BG-13
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
Overview of materials for Styrene-Butadiene Copolymer, SBC

PBLUST002 / 190978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.