MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips Sumika Marlex® AGM-010 Polypropylene; Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Polypropylene impact copolymer, cold temperature impact resistant.

Applications: Thermoformed parts, blow molded parts, and profile extrusion.

Information provided by Phillips

Meets FDA regulation CFR 177.1520 and may safely be used for articles in contact with food except for articles used for packing or holding food during cooking.

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccASTM D-1505
Melt Flow 1.0 g/10 min
@Temperature 230 °C
ASTM D-1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 86ASTM D-785
Hardness, Shore D 56ASTM D-2240
Tensile Strength, Yield 26.2 MPa50 mm/min; ASTM D-638
Flexural Modulus 1.17 GPaSecant, 1.3 mm/min; ASTM D-790
 1.31 GPaTangent, 13 mm/min; ASTM D-790
Izod Impact, Notched 60.0 J/m
@Temperature -30.0 °C
ASTM D-256
 NB
@Temperature 0.000 °C
ASTM D-256
 NB
@Temperature 23.0 °C
ASTM D-256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 97.0 °CASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °CASTM D-648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 350 - 380 °F
Middle Barrel Temperature 400 - 425 °F
Front Barrel Temperature 400 - 425 °F
Nozzle Temperature 400 - 425 °F
Mold Temperature 40.0 - 60.0 °F
Back Pressure 80.0 - 120 psi
 
Descriptive Properties
Manifold Temperature °F400-425
Parison Temperature °F395-410

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carmel Olefins Capilene® SL 50 Polypropylene Impact Copolymer
Carmel Olefins Capilene® TU 75 AV Polypropylene Impact Copolymer
Phillips 66 COPYLENE® CM360N Polypropylene, Impact Copolymer, Injection Molding
Phillips 66 COPYLENE® CM015 Polypropylene Impact Copolymer
Phillips 66 COPYLENE® CM005 Polypropylene Impact Copolymer

PCHEVD217 / 20711

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.