MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Vinnapas® 5012 T Vinyl Acetate-Ethylene Copolymer
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: Product description: VINNAPAS® 5012 T is a thixotropic, hard dispersible polymer powder based on vinyl acetate and ethylene for very good tensile adhesion strength.

Properties: VINNAPAS® 5012 T is a copolymer powder of vinyl acetate and ethylene and is dispersible in water. Compounds modified with VINNAPAS® 5012 T such as tile adhesives and troweling compounds, exhibit improved adhesion, flexural strength in bending, deformability and abrasion resistance and are easier to process. When used with cement and gypsum, it provides excellent non-sag properties. This is particularly useful for the production of vertical and overhead adhesives and wall-troweling compounds. VINNAPAS® 5012 T contains a fine mineral filler as an antiblocking agent. It is produced without the addition of organic solvents, plasticizers and film-forming agents.

Special features: VINNAPAS® 5012 T is a non-slump hard dispersible polymer powder. It has very good general-purpose properties in applications requiring mortars with nonslump properties. It is suitable for the formulation of mortars with low emissions.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.470 - 0.570 g/cc0.0170 - 0.0206 lb/in³DIN EN ISO 60
Solids Content >= 98 %>= 98 %
Particle Size 400 µm400 µmmax 4% over; DIN EN ISO 4610
Ash <= 13 %<= 13 %
 
Descriptive Properties
Appearancewhite to light beige powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWACK9605 / 205134

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.