MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 7701 Epoxy - Crowfoot Satin Fabric Composite
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC

Material Notes: Composite with E-Glass Fiber Reinforced Crowfoot Satin Fabric. CYCOM® 7701 resin is a 250°F (121°C) curing epoxy resin designed for use in structural laminates and honeycomb core sandwich panels for aircraft exteriors. In the prepreg form it has excellent drape and tack. CYCOM 7701 was created for autoclave fabrication; however, it can also be press molded and vacuum bag cured. The recommended lay-up procedure for CYCOM 7701 epoxy resin is L-3 or L-6. The recommended cure procedure is C-6 or C-7.

Features & Benefits:

  • 250°F (121°C) cure
  • 200°F (93°C) dry service temperature
  • Laminate and sandwich panel usage
  • Self-extinguishing and solvent resistant
  • Self-adhesive to honeycomb core
  • Autoclave, press mold or vacuum bag processing
  • Shelf life 6 months at 0°F (-18°C), 10 days at 72°F (22°C)
Applications: Structural laminates and honeycomb core sandwich panels for aircraft exteriors

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45000 - 51000 psi
@Temperature 82.0 °C
 56000 - 61000 psi
@Temperature -54.0 °C
 60000 - 63000 psi
@Temperature 24.0 °C
Tensile Modulus 16.0 - 18.0 GPa
@Temperature 82.0 °C
 17.0 - 19.0 GPa
@Temperature 24.0 °C
 19.0 - 21.0 GPa
@Temperature -54.0 °C
Compressive Strength 317 - 352 MPa
@Temperature 82.0 °C
 421 - 448 MPa
@Temperature -54.0 °C
 434 - 463 MPa
@Temperature 24.0 °C
Compressive Modulus 16000 - 18000 MPa
@Temperature 82.0 °C
 17000 - 19000 MPa
@Temperature 24.0 °C
 19000 - 21000 MPa
@Temperature -54.0 °C
Shear Strength 4700 - 4900 psi
@Thickness 610 mm
Interlaminar
 5000 - 5300 psi
@Thickness 2080 mm
Interlaminar
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 93.0 °Cdry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 250 °FCure Temperature
Shelf Life 0.333 Month
@Temperature 22.0 °C
 6.00 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Hexcel® HexPly® F155 Epoxy Resin
Hexcel® HexPly® M10E Epoxy Resin
Solvay CYCOM® 7668 Epoxy Resin
Evonik SILIKOPON® EF Silicone Epoxy Resin

PCYTED083 / 180385

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.