MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SMAC SMACMOUNT® 1224S Damping Material
Categories: Other Engineering Material

Material Notes: Specifications - Shock & vibration insulation for:
  • Ground & track vehicles
  • Embedded electronic
  • Shipboard equipment
  • Trays & racks systems
Advantages:
  • No special tools required
  • High damping isolators

Information provided by SMAC MontBlac Groupe Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 90.0 °C194 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Descriptive Properties
Frequency10-20 Hz
Load1 kg20 Hz, 0.9 mm, Natural Frequency
 1.2 kg20 Hz, 2.5 mm, Natural Frequency
 1.3 kg20 Hz, 5 mm, Natural Frequency
 1.5 kg4 mm, Static Deflection
 2.2 - 6.6 lbs
 3 kg9 Hz, 2.5 mm, Natural Frequency
 3 kg8 Hz, 0.9 mm, Natural Frequency
 3 kg9 Hz, 5 mm, Natural Frequency
 5.5 kg6 mm, Static Deflection
 9 kg10 mm, Static Deflection
MaterialsSMACSIL®
Metal partsStainless base plate, brass rivets
Overall size42.2 x 42.2 x 35.3 mm
Transmissibility at resonance<2.5
Weight78 g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SMAC SMACWRAP® ST Damping Material, 0.60 mm
SMAC SMACTANE® SP Damping Material
SMAC SMACSONIC® Classic ST Noise and Vibration Damping
SMAC CABLE® 2526S-20-08 Damping Material
SMAC CABLE® 2518S-10-08 Damping Material

PZSMAC018 / 146134

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.