MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Marco Polo MARPOL HDM 507 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: MARPOL® HDM 507 is a narrow molecular weight distribution copolymer resin that exhibits excellent toughness and impact strength. This is also designed for good stiffness and processability over a variety of molding conditions.

Recommended Applications: Industrial containers, pails, crates, cases and structural foam

FDA Status: Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.952 g/ccASTM D792
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2400 psiASTM D638
Tensile Strength, Yield 3000 psiASTM D638
Elongation at Break 700 %ASTM D638
Flexural Modulus 146000 psiASTM D790
2% Secant Modulus 146000 psiASTM D638
Izod Impact, Notched 1.20 ft-lb/in
@Temperature -50.0 °C
ASTM D256
 2.30 ft-lb/in
@Temperature -58.3 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 124 °CASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMARCO181 / 283778

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.