MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Rogers Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Side 1: Uncured Rubber
Side 2: Uncured Rubber

Appearance: Red silicone gum

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.50 milPolyethylene Interleave
 3.00 milPrime Coated 113 Fiberglass, Substrate
 6.00 - 8.00 milSide 1
 11.0 - 13.0 milOverall
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40 - 50Compound Property
Tensile Strength 855 - 1045 psiCompound Property
Elongation at Break 340 - 410 %Compound Property
Peel Strength >= 3.00 pli[ppi], Bond Strength
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength >= 400 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 450 °F
Minimum Service Temperature, Air -70.0 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 hour
@Temperature 232 °C
Recommended Postcure Cycle
 15.0 min
@Temperature 177 °C
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature <=23.9 °C
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)10 - 14
Uncoated Fabric Break Strength150 lb/inWarp Direction, Substrate Property
 70 lb/inFill Direction, Substrate Property

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Alcoa QC-10® Aluminum Mold Alloy
AISI 4130 Steel, annealed at 865°C (1585°F), furnace cooled 11°C (20°F)/hour to 680°C (1255°F), air cooled, 25 mm (1 in.) round
AISI 1020 Steel, cold rolled
Dura-Bar 65-45-12 Continuously Cast Ductile Iron Bar Stock ASTM A536

PARL219 / 125405

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.