MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kuraray Genestar™ GP2450NH-2 Nylon, 45% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Standard V-0 Grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm.

This grade meets UL94, V-0 Flammability rating without Chlorine and Bromine. It has good balance of mechanical properties and flow-ability as well as other V-0 grades containing Bromine Flame Retardant (BFR).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.53 g/cc1.53 g/cc
Water Absorption 0.80 %0.80 %
Linear Mold Shrinkage, Flow 0.00040 cm/cm0.00040 in/in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/in
Spiral Flow 5.50 cm
@Load 750 kg,
Temperature 320 °C
2.17 in
@Load 1650 lb,
Temperature 608 °F
0.5mm diameter
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 38.0 MPa5510 psiWeld; ASTM D638
 165 MPa23900 psiASTM D638
Elongation at Yield 0.40 %0.40 %Weld; ASTM D638
 3.0 %3.0 %ASTM D638
Flexural Strength 224 MPa32500 psiASTM D790
Flexural Modulus 13.0 GPa1890 ksiASTM D790
Izod Impact, Notched 1.00 J/cm1.87 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength 30.0 kV/mm762 kV/inASTM D149
Comparative Tracking Index >= 600 V>= 600 VASTM UL746A
 
Thermal PropertiesMetricEnglishComments
Melting Point 306 °C583 °F
Deflection Temperature at 1.8 MPa (264 psi) 285 °C545 °FASTM D648
Glass Transition Temp, Tg 125 °C257 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese VECTRA E130i LCP, 30% Glass Reinforced
Celanese VECTRA A130 LCP, 30% Glass Reinforced
Avient Edgetek® AM-45GF/000 PPA (Polyphthalamide), 45% Glass Fiber Reinforced, Hi-Temp
DuPont Mobility and Materials Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA)
DuPont Mobility and Materials Zytel® HTN 55G55LWSF BK752A Polyphthalamide (PPA)

PKUR120 / 162509

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.