MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes:
  • Hexene Linear Low Density Resin
  • Good Strength
  • High Output
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions)
TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designed for good strength and throughput rates. This product is recommended for thin and thick gauge applications such as consumer trash bags/liners and heavy duty shipping sacks that require toughness and output.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.932 g/ccASTM D792
Thickness 0.800 mil
Melt Flow 0.50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 3500 ppm
Slip Level 1200 ppm
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 3641 psiASTM D882
Film Tensile Strength at Yield, TD 3735 psiASTM D882
Film Elongation at Break, MD 530 %ASTM D882
Film Elongation at Break, TD 716 %ASTM D882
Secant Modulus, MD 0.2998 GPa2% Secant; ASTM D882
Secant Modulus, TD 0.3156 GPa2% Secant; ASTM D882
Impact 9.0[lbf]; Puncture Resistance Force; Dow Method
 158[ft-lbf/in3]; Puncture Resistance; Dow Method
 4414[ft-lbf/in3]; Toughness MD; ASTM D882
 5723[ft-lbf/in3]; Toughness TD; ASTM D882
Puncture Energy 19.0 in-lbDow Method
Elmendorf Tear Strength MD 332 gMethod B; ASTM D1922
Elmendorf Tear Strength TD 599 gMethod B; ASTM D1922
Elmendorf Tear Strength, MD 415 g/milASTM D1922
Elmendorf Tear Strength, TD 748.75 g/milASTM D1922
Dart Drop Test <= 100 gMethod B; ASTM D1709
 126 gMethod A; ASTM D1709
Film Tensile Strength at Break, MD 11373 psiASTM D882
Film Tensile Strength at Break, TD 10946 psiASTM D882
Heat Seal Strength, Ultimate 12.9 Nat 150°C, 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Heat Seal Strength Initiation Temperature 120 °C1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 126 °CDow Method (DSC)
Vicat Softening Point 119 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 13 %ASTM D1003
Gloss 46 %20°; ASTM D2457
 49 %45°; ASTM D2457
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin

PDOW1442 / 30660

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.