MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LG Chemical LUCON SP9306FL sPS+MF
Categories: Polymer; Thermoplastic; Polystyrene (PS); Syndiotactic Polystyrene (SPS)

Material Notes: Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat Resistance

Application: Electrical or Electronic Parts

CAS No. 9003-53-6, 65997-17-3, 68928-70-1 and 1309-64-4

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D792
Maximum Moisture Content 0.010Injection Molding
Linear Mold Shrinkage, Flow 0.0020 - 0.0080 cm/cm
@Thickness 3.20 mm
ASTM D955
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 290 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 1200 kg(f)/cm²
@Thickness 3.20 mm
5mm/min; ASTM D638
Flexural Yield Strength 1800 kg(f)/cm²
@Thickness 6.40 mm
1.3mm/min; ASTM D790
Flexural Modulus 1800 kg(f)/cm²
@Thickness 6.40 mm
1.3mm/min; ASTM D790
Izod Impact, Notched 7.00 kg-cm/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Surface Resistance 1.00e+15 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.400 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 220 °C
@Thickness 6.40 mm
ASTM D648
UL RTI, Electrical 125 °C
@Thickness >=1.60 mm
 130 °C
@Thickness >=3.00 mm
UL RTI, Mechanical with Impact 115 °C
@Thickness >=1.60 mm
 120 °C
@Thickness >=3.00 mm
UL RTI, Mechanical without Impact 125 °C
@Thickness >=1.60 mm
 130 °C
@Thickness >=3.00 mm
Flammability, UL94 V-0
@Thickness >=1.60 mm
 V-0
@Thickness >=3.00 mm
 5VA
@Thickness >=1.60 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 300 °CInjection Molding
Middle Barrel Temperature 270 - 320 °CInjection Molding
Front Barrel Temperature 275 - 320 °CInjection Molding
Nozzle Temperature 315 °CInjection Molding
Melt Temperature 315 °CResin, Injection Molding
Mold Temperature 80.0 - 130 °CInjection Molding
Drying Temperature 120 - 140 °CInjection Molding
Dry Time 3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPaInjection Molding
Screw Speed 40 - 60 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Edgetek® QT-30GF/000 Natural Syndiotactic Polystyrene (SPS)
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
Avient Edgetek® QT020GFS/000 FR NATURAL Syndiotactic Polystyrene (SPS)
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
I. Stern GPPS-004 General Purpose Crystal Polystyrene

PLAY269 / 148279

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.