MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Latrobe Dynaflex® VAC-ARC High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Medium Alloy Steel

Material Notes: DYNAFLEX VAC-ARC steel is a medium alloyed, air hardening ultra high strength grade designed for structural applications requiring room temperature tensile strengths of 220,000 to 300,000 psi. Due to the secondary hardening feature exhibited by this alloy, stable elevated temperature properties are available up to

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.282 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 260 ksi
Tensile Strength, Yield 1585 MPa
@Strain 0.2 %
<150 in2
Reduction of Area 6.0 %
Modulus of Elasticity 30000 ksi
 23000 ksi
@Temperature 538 °C
 27000 ksi
@Temperature 204 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.5 µm/m-°C
@Temperature 21.0 - 204 °C
 13.1 µm/m-°C
@Temperature 21.0 - 648 °C
Specific Heat Capacity 0.110 BTU/lb-°F
@Temperature 0.000 - 100 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 815 °CCritical Temperaure
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.40 %
Chromium, Cr 5.0 %
Iron, Fe 91.6 %
Manganese, Mn 0.30 %
Molybdenum, Mo 1.3 %
Silicon, Si 0.90 %
Vanadium, V 0.50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ASTM A553 Alloy Steel, Grade II
ASTM A553 Alloy Steel, Grade I
ASTM A844 Alloy Steel
AISI Type S1 Tool Steel, quenched 955°C (1750°F), tempered 150°C (300°F)
AISI Type S2 Tool Steel, austenitized 845°C (1550°F), brine quenched to 35 HRC

NTIMK045 / 19392

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.