MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 12.7 - 25.4 mm.
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Ampco 483 alloy will maintain mechanical properties at temperatures up to 315ºC and has a machinability rating of 20%. The alloy provides excellent corrosion resistance to sea water and non-oxidizing mineral acids. Can be welded with both the gas-shielded and shielded metal-arc processes. Brazing, soldering and oxyfuel gas welding are not recommended. Ampco 483 alloy can be hot worked at temperatures from 705º to 926ºF and annealed between 705º and 880ºF. The alloy has a forgeability rating of 75%. The consistent superiority of Ampco 483 alloy over commercial bronze is due, in large part, to the unique distribution of alloy microstructure, often referred to as the Ampco-Phase. Only Ampco alloys offer this metallurgical advantage.

Applications: Uses include: cams; bushings; bearing retainer cages; valve stems and guides; sleeve bearings.

Key Words: ASTM B124; ASTM B150; Federal QQ-C-00465
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.64 g/cc
Density 7.64 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 212HB 30
Hardness, Rockwell B 96
Tensile Strength, Ultimate >= 605 MPa
Tensile Strength, Yield >= 305 MPa
Elongation at Break >= 18 %
Tensile Modulus 117 GPa
Modulus of Rigidity 44.0 GPa
Compressive Yield Strength 117 MPaProportional Limit
Compressive Strength 758 MPa
Poissons Ratio 0.32
 0.33Calculated
Shear Modulus 44.0 GPacalculated
Charpy Impact 13.0 - 16.0 JKeyhole
 23.0 - 27.0 JV-notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000246 ohm-cm
@Temperature 20.0 °C
7% I.A.C.S.
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.440 J/g-°C
Thermal Conductivity 36.0 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 9.0 %
Copper, Cu 81 %
Iron, Fe 3.0 %
Manganese, Mn 1.5 %
Nickel, Ni 5.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nickel Aluminum Bronze, UNS C63000, HR50 Temper
Aluminum Bronze, UNS C95400, Copper Casting Alloy, TQ50 Temper
Ampco Metal AMPCO® 483 Aluminum-Nickel Bronze, Extruded Rod, 25.4 - 50.8 mm.
Chicago Extruded Metals BioBrass® UNS C62300 Aluminum Bronze
Chicago Extruded Metals BioBrass® UNS C62400 Aluminum Bronze

NAMPCO26 / 14980

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.