MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Resinlab® UR3001 Clear Two Part Urethane Encapsulant
Categories: Polymer; Adhesive; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: Resinlab™ UR 3001 is a clear, two component, room temperature curing urethane encapsulating system. It is designed to cure completely at room temperature. UR 3001 provides excellent environmental protection while having tenacious adhesion to various metals, plastics and other common assembly materials. UR 3001 is an unfilled system that has a gel-like durometer and good flexibility at temperatures as low as –40°C. It provides excellent moisture resistance and can withstand 125°C continuous operation. UR 3001 has a convenient mixing ratio of 2 to 1 by volume. It is well suited to automated meter mix operations. UR 3001 is a DOT non-hazardous material and contains no TDI, MOCA, or other reportable substances. Part B is moisture sensitive and must be kept away from atmospheric moisture during storage. After opening a sealed container, thoroughly purge the remaining air space with dry nitrogen (or equivalent) before closing the container.

Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 g/ccPart A
 0.940 g/ccMixed
 0.990 g/ccPart B
Viscosity 75 cPPart B
 1500 cPMixed
 3750 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 psi
Elongation at Break >= 135 %
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
Dielectric Constant 3.6
@Frequency 100 Hz,
Temperature 25.0 °C
Dielectric Strength 380 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°C
Maximum Service Temperature, Air 125 °C
 150 °C
Minimum Service Temperature, Air -40.0 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %clear; thickness not quantified
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 85.0 °C
 24.0 hour
@Temperature 25.0 °C
Pot Life 10 minMass: 50g
 
Descriptive Properties
ColorClear
Mix Ratio2:1Weight and Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotchkote™ 60EG 533 Urethane Elastomer
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel
Northstar Polymers MPC-W44A Polyurethane Gel
Northstar Polymers GK-7 Low Viscosity Polyurethane Gel Cast
Freudenberg Hydrolysis-Resistant Polyurethane Elastomer

PRESL187 / 101601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.