MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Oceanchem Group Antioxidant 1024
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Molecular Formula: C34H52N2O4

Uses: Dosage is 0.1-0.5 portions. It is a metal deactivator, can work with antioxidant, used in PE, PP, polystyrene, polyamnamee, polyester, or used as antioxidant of bakelite, wire and cable.

Storage and Packing: Stored in a dark and dry place in room temperature, plastic bag lined carton.

Information Provided by Oceanchem Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.50 %
Molecular Weight 553 g/mol
Ash <= 0.10 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 224 - 229 °C
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 96 %
@Wavelength 425 nm
toluene solution
 98 %
@Wavelength 500 nm
toluene solution
 
Descriptive Properties
AppearanceWhite crystalline powder
Assay (%)>99
Molecular FormulaC34H52N2O4
Solubility0.1%toluene (25°C, Wt)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Parker Chomerics CHO-BOND® 1024 Conductive Silicone Splicing Compound
Evonik VESTOWAX® SP 1024 Fischer-Tropsch Wax
A. Schulman BMC HT12-1024 Automotive Grade Molding compound

POCEAN51 / 104255

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.