MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Excel Industries PROXEL™ GXL Antimicrobial
Categories: Other Engineering Material

Material Notes: PROXEL GXL is a broad spectrum biocide for the preservation of industrial water-based products against spoilage from bacteria, yeasts and fungi. PROXEL GXL is a 20% aqueous dipropylene glycol solution of 1,2-benzisothiazolin-3-one.

Applications: PROXEL GXL is effective in a wide range of industrial aqueous-based products. Application areas include:

  • Synthetic polymer emulsions
  • Emulsion paints
  • Water-based adhesives
  • Household products
  • Printing inks
  • Paper coating compositions
  • Metal working fluids
  • Agricultural pesticide dispersions
  • Aqueous mineral and pigment slurries
  • Tape joint compounds
  • Leather processing solutions

Information provided by Excel Industries Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/cc
pH 13.513.5
Viscosity  400 cP
@Temperature 25.0 °C
400 cP
@Temperature 77.0 °F
 2000 cP
@Temperature 10.0 °C
2000 cP
@Temperature 50.0 °F
 
Thermal PropertiesMetricEnglishComments
Boiling Point 100 °C212 °F
 
Descriptive Properties
Physical stateYellow-light brown solution

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEXCEL019 / 183495

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.