MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polymer Resources NY6-GP2-[color]-H General Purpose Nylon 6, Nucleated, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized; Nylon 6, Unreinforced

Material Notes: General Purpose Nylon 6, Nucleated, Heat Stabilized

Process: Injection Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).

Information provided by Polymer Resources Corporation.

Key Words: UL E113219
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.13 g/cc1.13 g/ccASTM D792
Linear Mold Shrinkage 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 89.6 MPa13000 psiASTM D638
Tensile Strength, Yield 89.6 MPa13000 psiASTM D638
Flexural Strength 108 MPa15700 psiASTM D790
Flexural Modulus 3.10 GPa450 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Temperature 22.8 °C
1.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Gardner Impact 36.2 J26.7 ft-lbASTM D3029
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmASTM D257
Dielectric Strength 29.9 kV/mm760 kV/inASTM D149
Comparative Tracking Index >= 600 V>= 600 VUL 746
Hot Wire Ignition, HWI  7.0 - 15 sec
@Thickness 0.800 mm
7.0 - 15 sec
@Thickness 0.0315 in
UL 746
 7.0 - 15 sec
@Thickness 1.50 mm
7.0 - 15 sec
@Thickness 0.0591 in
UL 746
 15 - 30 sec
@Thickness 3.00 mm
15 - 30 sec
@Thickness 0.118 in
UL 746
 30 - 60 sec
@Thickness 5.99 mm
30 - 60 sec
@Thickness 0.236 in
UL 746
High Amp Arc Ignition, HAI  >= 120 arcs
@Thickness 0.800 mm
>= 120 arcs
@Thickness 0.0315 in
UL 746
 >= 120 arcs
@Thickness 1.50 mm
>= 120 arcs
@Thickness 0.0591 in
UL 746
 >= 120 arcs
@Thickness 3.00 mm
>= 120 arcs
@Thickness 0.118 in
UL 746
 >= 120 arcs
@Thickness 5.99 mm
>= 120 arcs
@Thickness 0.236 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min0.394 - 1.00 in/minUL 746
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 191 °C375 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C165 °FASTM D648
UL RTI, Electrical  125 °C
@Thickness 0.800 mm
257 °F
@Thickness 0.0315 in
UL 746
 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746
 125 °C
@Thickness 3.00 mm
257 °F
@Thickness 0.118 in
UL 746
 125 °C
@Thickness 5.99 mm
257 °F
@Thickness 0.236 in
UL 746
UL RTI, Mechanical with Impact  65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
UL 746
 85.0 °C
@Thickness 1.50 mm
185 °F
@Thickness 0.0591 in
UL 746
 85.0 °C
@Thickness 3.00 mm
185 °F
@Thickness 0.118 in
UL 746
 85.0 °C
@Thickness 5.99 mm
185 °F
@Thickness 0.236 in
UL 746
UL RTI, Mechanical without Impact  65.0 °C
@Thickness 0.800 mm
149 °F
@Thickness 0.0315 in
UL 746
 75.0 °C
@Thickness 1.50 mm
167 °F
@Thickness 0.0591 in
UL 746
 75.0 °C
@Thickness 3.00 mm
167 °F
@Thickness 0.118 in
UL 746
 75.0 °C
@Thickness 5.99 mm
167 °F
@Thickness 0.236 in
UL 746
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 221 - 246 °C430 - 475 °F
Middle Barrel Temperature 238 - 254 °C460 - 490 °F
Front Barrel Temperature 243 - 260 °C470 - 500 °F
Melt Temperature 238 - 279 °C460 - 535 °F
Mold Temperature 79.4 - 93.3 °C175 - 200 °F
Drying Temperature 73.9 - 85.0 °C165 - 185 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Vent Depth 0.000762 cm0.000300 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYQ073 / 160589

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.