Nipol 1000X132 is a copolymer of butadiene and acrylonitrilewith extremely high fuel and oil resistance. Sufficient antioxidant is added duringmanufacture for normal storage conditions. Ultra-high ACN level for maximum oil and fuel resistance and low gas permeability |