MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay CYCOM® 934 Epoxy Prepreg Neat Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: CYCOM® 934 is a high flow, 350°F (177°C) curing epoxy resin with good 200°F (93°C) wet and 350°F (177°C) dry service capability. CYCOM 934 is formulated for autoclave processing, but it has been successfully processed by press molding. Unidirectional tape and woven fabric impregnated with CYCOM 934 resin will retain good tack and drape for at least 10 days at 70°F (21°C). Standard cure is for two hours at 350°F (177°C). No post cure is required for 350°F (177°C) dry service capability. CYCOM 934 can be impregnated via hot melt or solution techniques on all available fibers and fabrics.

Features & Benefits:

  • Available in a broad range of fibers and forms including tape, fabric and roving
  • Large industry database
  • Widely used in aerospace, commercial and military structural applications
  • Laminate and sandwich panel usage
  • Autoclave or press-mold processing
  • Shelf life of 6 months at 0°F (-18°C), 10 days at 72°F (22°C)
  • Meets all NASA outgassing requirements

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 12000 psi
Elongation at Break 0.70 %
Flexural Strength 10000 psi
@Temperature 23.0 °C
 10000 psi
@Temperature 93.0 °C
Wet
 17000 psi
@Temperature 93.0 °C
Flexural Modulus 2.80 GPa
@Temperature 93.0 °C
Wet
 3.20 GPa
@Temperature 93.0 °C
 4.10 GPa
@Temperature 24.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °FWet
 350 °FDry
Glass Transition Temp, Tg 160 °CWet
 194 °CDry
 
Processing PropertiesOriginal ValueComments
Processing Temperature 350 °F
@Time 7200 sec
Standard Cure
Shelf Life 0.333 Month
@Temperature 22.2 °C
 6.00 Month
@Temperature -17.8 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M55J Fiber
Hexcel® HexPly® 8551-7 Epoxy Matrix
Hexcel® HexPly® 954-3 Curing Cyanate Resin, M55J Fiber
Hexcel® HexPly® 954-3A Curing Cyanate Resin, M55J Fiber
Hexcel® HexPly® M65 Bismaleimide Resin

PCYTED096 / 180398

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.