XT polymer X800RG compound is an impact-modified acrylic-based multipolymer for molding, extrusion and blow molding applications. Typical properties of XT polymer compounds are:- outstanding thermoformability
- superior heat distortion temperatures
- excellent bonding and welding capabilities
- good impact strength
- good light transmission
- resistant to EtO, gamma and E-beam sterilization
- resistant to PVC plasticizers
The special property of XT polymer 375 compund is- high melt flow rate
- good chemical resistance
Application: Used for food packaging and appliance partsInformation Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm (Roehm) GmbH. |