MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Grade 1250 Ceramic fiber paper
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Pyrotek Grade 1250 ceramic fiber paper is manufactured under carefully controlled conditions from high purity fibers to ensure close thickness tolerance and uniformity of density. The product contains a non-toxic, low smoke emission binder.

Applications

  • Launder lining back-up
  • Launder gaskets
  • Mold lining
  • Furnace seals

Advantages

  • High handling strength
  • Easy to cut or wrap
  • Good insulation properties
  • Good thermal shock resistance

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.220 g/cc0.00795 lb/in³
Binder 0.0500.050organic
 
Thermal PropertiesMetricEnglishComments
Melting Point 1760 °C3200 °F
Maximum Service Temperature, Air 1250 °C2280 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator

CPYRO139 / 1860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.