MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CLAL-MSX ARCAP Anticorrosion AP1 0 Annealed, Rolled Copper Alloy
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Description: The AP1D grade has been developed especially for being machined by lathe. The very good machineability of the AP1D grade may be summerised by: cutting speed up to 150 m/minute (according to the type of part, cutting tool and lathe), very good quality of surface that can be lapped or polished with a diamond tool, burr free after drilling, and reduction in frequency of tool sharpening.

High Corrosion Resistance: ARCAP alloys are very corrosion resistant to the majority of chemical and physical environments. CLAL can provide data for the corrosion resistance of ARCAP alloys. In particular ARCAP alloys have a very high resistance to scaling and clogging of pipes by hard water and the blocking of pipes used for transport powder products such as sodium aluminate, cement, etc.

High Mechanical Properties: In annealed temper ARCAP, alloys have an elongation up to 45 %, which allows deep drawing. In spring temper the ultimate tensile strength is above 800 MPa.

Non-Magnetic: A detector sensitive to 1/10 of nanotesla, placed at less than 1 mm from ARCAP alloys will not show any magnetic interference. This non magnetism is kept even at very low temperatures (measured at 4.2° k).

Stable Resistivity: Temperature variations have almost no effect on the resistivity of ARCAP alloys. The temperature coefficient of the grade AP4 is 4 x 10-5/°C and 25 x 10-5/°C for the other grades.

Excellent Behaviour At Low Temperature: At low temperatures the mechanical properties of ARCAP alloys are improved. A cryogenic application shows that the ultimate tensile strength and the yield strength increase without any diminution of the elongation or the impact strength.

Very Easy To Process: ARCAP alloys are easily processed whether by forging, stamping, deep drawing, machining, welding or brazing. They are also easily plated.

Information provided by CLAL-MSX

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.80 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers <= 120
Tensile Strength, Ultimate <= 400 MPa
Tensile Strength, Yield <= 300 MPa
@Strain 0.2 %
Elongation at Break >= 30 %LO=50 mm
Modulus of Elasticity 163 - 170 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000351 - 0.0000400 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 0.000 - 300 °C
 17.0 µm/m-°C
@Temperature 0.000 - 600 °C
Thermal Conductivity 22.0 W/m-K
@Temperature <=20.0 °C
 25.0 W/m-K
@Temperature <=200 °C
Melting Point 1150 - 1170 °C
Solidus 1150 °C
Liquidus 1170 °C
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) 0.70Relative to Silver = 1
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 65 %
Nickel, Ni 25 %
Other 2.0 %
Zinc, Zn 8.0 %
 
Descriptive Properties
ColorWhiteish bluish
Non Magnetism request1E-05 Oersted
Temperature Coefficient0.00025K-1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics SSN Sintered Silicon Nitride Mac-SSNS
Special Metals INCONEL® 706 Precipitation Hardening Alloy, Cold Rolled Sheet, Solution Treated
AK Steel Full Hard Only, Grade 80 Cold Rolled Carbon Steel, Structural Steel (SS)
ArcelorMittal MartINsite® 1200 Cold Rolled Steel
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 30% Cold Rolled (UNS S30400)

NCLAL001 / 160032

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.