MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Silon TABOREX TA 1160 CL Chemically-Crosslinkable HDPE Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Crosslinkable (XLPE)

Material Notes: TABOREX TA 1160 CL is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a TABOREX Masterbatch containing the crosslinking catalyst a “SIOPLAS-SYSTEM”. Pipes which are produced with the SILON grade TABOREX TA 1160 CL fulfill the requirements of ASTM F876, CSA 137.5, EN ISO 15875, BS 7291 and all related standards. This system allows the compound to be extruded as a normal thermoplastic polymer and will attain a high level of crosslinking in the processed form. The final product provides all the superior properties associated with crosslinked polyethylene.

Information provided by Silon US LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.530 g/ccISO 60
Density 0.948 g/ccISO 1183-1
Volatiles <= 0.250 %CSN 640311
Moisture Absorption <= 0.0200 %ISO 15512
Melt Flow 1.60 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 24.0 MPaISO 527
Elongation at Break 450 %ISO 527
 
Processing PropertiesOriginal ValueComments
Zone 1 160 - 170 °C
Zone 2 170 - 180 °C
Zone 3 170 - 190 °C
Zone 4 170 - 190 °C
Die Temperature 190 - 220 °C
Head Temperature 200 - 210 °F
Shelf Life 9.00 Month
@Temperature <=30.0 °C
 
Descriptive Properties
Gel content (%)72ISO 10147
Screw Compression ratio2.5-3:1
Screw L/D>25
Screw Temperature70-90°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSILOM9803 / 325129

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.