MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Flam™ 205 HFRI Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:

Features:

  • Flame Retardant
  • Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 1.34 g/ccASTM D792
    Linear Mold Shrinkage 0.0090 cm/cmASTM D955
    Melt Flow 4.0 g/10 min
    @Load 2.16 kg,
    Temperature 230 °C
    ASTM D1238
     
    Mechanical PropertiesOriginal ValueComments
    Tensile Strength, Ultimate 2200 psiASTM D638
    Elongation at Break 10 %ASTM D638
    Flexural Strength 3000 psiASTM D790
    Flexural Modulus 250000 psiMethod I (3 point load), Procedure B); ASTM D790
    Izod Impact, Notched 5.00 ft-lb/inASTM D256
    Gardner Impact 14.00 ft-lbASTM D3029
     
    Thermal PropertiesOriginal ValueComments
    Deflection Temperature at 0.46 MPa (66 psi) 169 °FUnannealed; ASTM D648
    Deflection Temperature at 1.8 MPa (264 psi) 149 °FUnannealed; ASTM D648
    Vicat Softening Point 248 °FASTM D1525
    Flammability, UL94 V-0
    @Thickness 1.59 mm
     V-0
    @Thickness 3.17 mm
    Oxygen Index 26 %ASTM D2863

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Plastcom SLOVALEN PH 78 FRT 5 Polypropylene Homopolymer, Halogen Free and Phosphor Free Flame Retardant
    Plastcom SLOVALEN PH 76 FRD 3 PP, flame retardant
    Multibase Multi-Flam™ 0206 PP Polypropylene
    Multibase Multi-Flam™ 0220 PP Polypropylene
    Multibase Multi-Flam™ 0302 PP NH Polypropylene

    PMULTI289 / 54193

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.