MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene GA502119 Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade

Material Notes: The Petrothene GA502 series of resins are pelletized linear low density polyethylenes for applications requiring excellent drawdown and toughness. These pelletized products offer excellent additive homogeneity, require no transfer equipment modification and facilitate clean and safe storage and handling. They can be used in either blown or cast film extrusion. GA502119 is formulated without TNPP. Applications: Bags & Pouches, Can Liners, Color Concentrates, Film Wrap, Food Packaging Film, Lamination Film, Liner Film, Stretch Wrap Film

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Base Resin Density 0.918 g/ccASTM D1505
Density 0.918 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 0.000 ppmLYB Method
Slip Level 0.000 ppmLYB Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 750 %ASTM D882
Film Elongation at Break, TD 800 %ASTM D882
Elmendorf Tear Strength MD 170 gASTM D1922
Elmendorf Tear Strength TD 400 gASTM D1922
Dart Drop Test 120 gF50; ASTM D1709
Film Tensile Strength at Break, MD 33.8 MPaASTM D882
Film Tensile Strength at Break, TD 24.8 MPaASTM D882
1% Secant Modulus, MD 221 MPaASTM D882
1% Secant Modulus, TD 248 MPaASTM D882
 
Descriptive Properties
Processing MethodBlown Film, Cast Film, Compounding
Test Specimen1.5 mil gauge, 2.1:1 BUR

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene

PEQT8820 / 220454

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.