Description POLYBATCH® 2600V is a yellow color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 2600V contains heavy metal pigment(s) and is typically recommended for use at 5% addition levels.
Information provided by A. Schulman. |