MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Hexcel® HexPly® 924 180°C Curing Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: HexPly® 924 is a controlled flow epoxy matrix developed for the fabrication of high temperature resistant primary structures. When cured, HexPly® 924 becomes a tough composite with high impact resistance and damage tolerance. It is particularly suitable for aircraft primary structures and elevated temperature applications such as performance cars.
HexPly® 924 is best suited to autoclave or press cure to obtain optimum mechanical performance from the cured composite.

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccCured
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 65.0 MPaISO R527 type 1
Elongation at Yield 2.4 %ISO R527 type 1
Tensile Modulus 3.80 GPaISO R527 type 1
Flexural Yield Strength 120 MPaISO 178
Flexural Modulus 3.12 GPaISO 178
Compressive Strain at Yield 13 %ISO 604
Compressive Yield Strength 175 MPaISO 604
Poissons Ratio 0.41ISO R527 type 1
Fracture Toughness 0.830 MPa-m½
Shear Modulus 1.34 GPaISO R527 type 1
Toughness 150 JPer square meter
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 190 °CDMTA
Shrinkage 1.6 %
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
@Temperature -18.0 °C
 
Descriptive Properties
Tack Life (days)21

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® F263 Epoxy Resin
Hexcel® HexPly® F185 Epoxy Resin
Hexcel® HexPly® F155 Epoxy Resin
Hexcel® HexPly® 922-1 180°C Curing Epoxy Matrix
Hexcel® HexPly® EH25 180°C Curing Epoxy Matrix

PHEXC068 / 98538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.