MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Teknor Apex HFFR 2005 Polyolefin, Halogen Free
Categories: Polymer; Thermoplastic; Polyolefin; Polyolefin, Wire/Cable Grade

Material Notes: Notes: RoHS Compliant

Features: Flame Retardant; Halogen Free

Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable Jacketing

Agency Ratings: IEC Unspecified Rating; ICEA Unspecified Rating; UL QMTT2 .E200337

Processing Method: Extrusion

Forms: Pellets

Additional Information:

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 100°C: 78%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 100°C: 113%

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 113°C: 74%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 113°C: 108%

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 125°C: 73%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 125°C: 116%

Ultimate Elongation Retained, UL 1581, Oven Aged, 7 days, 136°C: 72%

Tensile Strength Retained, UL 1581, Oven Aged, 7 days, 136°C: 109%

Acid Gas, MIL-C-24643: < 5.0 mg

Acidity of Gases, IEC-754-2: < 6.0 pH

Conductivity: < 2.0 µS/cm

Smoke Index, NES-711: < 10.0

Toxicity Index, NES-713: 0.085

Acid Gas, MIL-C-24643: < 5.0 mg

Acidity of Gases, IEC-754-2: < 6.0 pH

Conductivity: < 2.0 µS/cm

Smoke Index, NES-711: < 10.0

Toxicity Index, NES-713: < 1.0

Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 154 kW/m2

Cone Calorimeter at 50 kW/m2, Total Heat Released: 157 MJ/m2

Cone Calorimeter at 50 kW/m2, Peak Smoke: 0.8 1/m

Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 138 sec

Information Provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.49 g/ccASTM D792
Melt Flow 1.5 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5310 seconds; ASTM D2240
Tensile Strength at Break 2070 psiASTM D638
Elongation at Break 140 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 9.70e+14 ohm-cmASTM D257
Dielectric Constant 3.66
@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature -40.0 °FASTM D746
Oxygen Index 44 %ASTM D2863
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNO597 / 128775

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.