MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 4002 Polyphthalamide (PPA), Glass Fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D 792
Water Absorption 0.25 %
@Time 86400 sec
ASTM D 570
Additive Loading 15 %Primary Additive
Linear Mold Shrinkage 0.0050 cm/cm
@Thickness 3.20 mm
ASTM D 955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 125ASTM D 785
Tensile Strength at Break 16000 psiASTM D 638
Elongation at Break 1.0 - 2.0 %ASTM D 638
Tensile Modulus 1200 ksiASTM D 638
Flexural Strength 23000 psiASTM D 790
Flexural Modulus 1100 ksiASTM D 790
Izod Impact, Notched 1.00 ft-lb/in
@Thickness 3.20 mm
ASTM D 256
Izod Impact, Unnotched 10.0 ft-lb/in
@Thickness 3.20 mm
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D 257
Dielectric Constant 5.0
@Frequency 1e+6 Hz
Dry; ASTM D 150
Dielectric Strength 520 V/milShort Term; In Oil; ASTM D 149
Dissipation Factor 0.019
@Frequency 1e+6 Hz
Dry; ASTM D 150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 µin/in-°FE 831
Deflection Temperature at 1.8 MPa (264 psi) 450 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 575 - 625 °F
Mold Temperature 275 - 325 °F
Drying Temperature 225 °F
@Time >=14400 sec
Moisture Content 0.050 %
Dew Point -25.0 °F
Injection Pressure 10000 - 18000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latilub 57D-15T G/30 PPA, 30% Glass Fiber Reinforced
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Eurotec® Tecomid® NT40 GR30 NL HS PPA, 30% glass fiber reinforced, heat stabilized, natural
Eurotec® Tecomid® NT40 CR30 BK111 HS PPA, 30% carbon fiber reinforced, heat stabilized, natural
E-Polymers SEPAZ® V330HS 30% Glass Fiber Reinforced Heat Stabilized PPA

PQZWA3163 / 91574

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.