MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Delrin Delrin® RAFG500P NC010 POM, Renewably Sourced
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Homopolymer, Unreinforced

Material Notes: Medium Viscosity Renewable Attributed Acetal Homopolymer Developed for Food Contact Applications

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccISO 1183
Water Absorption 1.4 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.400 %
@Thickness 2.00 mm
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.019 cm/cmISO 294-4, 2577
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 190 °C
cm³/10min Volumetric; ISO 1133
 15 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 92ISO 2039-2
Hardness, Rockwell R 120ISO 2039-2
Tensile Strength, Yield 71.0 MPaISO 527-1/-2
Elongation at Break 30 %Nominal; ISO 527-1/-2
Elongation at Yield 17 %ISO 527-1/-2
Tensile Modulus 3100 MPaISO 527-1/-2
Flexural Strength 80.0 MPa
@Strain 3.5 %
ISO 178
Flexural Modulus 2900 MPaISO 178
Poissons Ratio 0.37
Izod Impact, Notched (ISO) 8.00 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched 280 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 300 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2800 MPa1h; ISO 899-1
Tensile Creep Modulus, 1000 hours 1600 MPa1000h; ISO 899-1
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 110 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 110 µm/m-°CISO 11359-1/-2
Melting Point 178 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 158 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °CISO 75-1/-2
Vicat Softening Point 155 °C50°C/h, 50N; ISO 306
Flammability, UL94 HB
@Thickness 0.750 mm
IEC 60695-11-10
 HB
@Thickness 1.50 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Melt Temperature 215 °COptimum, Injection
 210 - 220 °CRange, Injection
Mold Temperature 90.0 °COptimum, Injection
 80.0 - 100 °CInjection
Drying Temperature 80.0 °CInjection
Dry Time 2.00 - 4.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.20 %Injection
Hold Pressure 80.0 - 100 MPaInjection
 100 MPaInjection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)3.1VDA 277
Emissions (mg/kg)<8VDA 275
Fogging (%)90F-value (refraction); ISO 6452
Fogging (mg)0.35G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.3Injection
PolymerPOM
Processing Hold Pressure Time (s/mm)8Injection
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5155f / 290912

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.