MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Fibre Glast 72 White Gel Coat  (discontinued **)
Categories: Polymer; Thermoset

Material Notes: Description:

#72 is the industry production standard for molding applications. Use as a sandable base coat for painting or polish to a high luster finish. Spray unthinned into molds using a cup gun or blend with Hi-Gloss Additive when performing repairs. Can be tinted with color pigments as needed, changing bold colors into pastels. #72 is a high quality coating developed for use in the fiberglass industry. This gel coat yields a quality finish, with good chemical/water resistance, gloss retention, weatherability, and resiliency. An un-tinted straight white gel coat, #72 is in the color match "C" category, meaning that batch to batch color variation can occur.
#72 White Gel Coat is formulated to meet the rigid requirements of transportation, boating, and sanitary applications. It has enabled customers to meet and surpass all requirements of the American National Standard for plastic bath tubs, shower receptors and shower stalls. ANSI Z 124.1, .2-1995, Sec. 6.1.1.
#72 White Gel Coat is ready to use, easy to spray, sag resistant, fast curing and requires only the addition of the proper amount of #69 Methyl Ethyl Ketone Peroxide to cure.
  • 36% Volatile Organic Compounds
  • Lay up time: 45 - 60 minutes
  • Sag Resistance: Good at 20 mils
  • Complete hide at 8 - 13 mils
  • Color Match CMC maximum DE of 1 unit

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 16000 - 20000 cPBrookfield RVF #4 Spindle at 4 rpm
 
Thermal PropertiesOriginal ValueComments
Flash Point 82.0 °F
 
Processing PropertiesOriginal ValueComments
Gel Time 10.5 - 16.5 minValue at 77°F with 1.8% MEKP

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Gypsum (CaSO4 - 2H2O)
Calcium Sulfate Dihydrate, CaSO4-2H2O
Abatron ClearStrip™ Stripper for Paint, Varnish, Coatings; Gel
Titanium Dioxide, TiO2, Anatase
Titanium Dioxide, Rutile

PFIBRE36 / 38299

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.