MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Elliott Company ELFOAM® P400 Polyisocyanurate Foam
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane Foam, Unreinforced

Material Notes: ELFOAM P400 is a 4.0 lb/ft3 (64 kg/m3), rigid, unfaced, closed cell polyisocyanurate foam supplied as blocks, sheets, shapes and custom parts for a variety of insulation, core material and carving applications. Polyisocyanurate foam (polyiso) is similar to polyurethane foam but offers greater dimensional stability over a wider service temperature range.

Applications include:

  • Laminated wall and roof panels
  • Truck bodies, trailers, shipping containers and railcars
  • FRP panels, tanks and shelters
  • Pultrusion and infusion processes
  • Plugs, patterns and carved products

Information provided by Elliott Company of Indianapolis Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0640 g/cc0.00231 lb/in³ASTM D1622
Water Absorption 0.50 %0.50 %By Volume; ASTM C272
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.407 MPa>= 59.0 psiPerpendicular; ASTM D1623
 0.552 MPa80.0 psiParallel; ASTM D1623
Tensile Modulus >= 0.0108 GPa>= 1.56 ksiPerpendicular; ASTM D1623
 0.0186 GPa2.70 ksiParallel; ASTM D1623
Compressive Strength >= 0.427 MPa>= 62.0 psiPerpendicular; ASTM D1621
 0.586 MPa85.0 psiParallel; ASTM D1621
Compressive Modulus >= 0.00965 GPa>= 1.40 ksiPerpendicular; ASTM D1621
 0.0145 GPa2.10 ksiParallel; ASTM D1621
Shear Modulus >= 0.00517 GPa>= 0.750 ksiPerpendicular; ASTM C273
 0.00586 GPa0.850 ksiParallel; ASTM C273
Shear Strength >= 0.345 MPa>= 50.0 psiPerpendicular; ASTM C273
 0.379 MPa55.0 psiParallel; ASTM C273
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C
@Temperature -17.8 - 121 °C
35.0 µin/in-°F
@Temperature 0.000 - 250 °F
ASTM E228
Insulation R Value 5.45.4Hr-ft²-°F/BTU; Aged 10 days at 158°F; ASTM C518
 5.95.9Hr-ft²-°F/BTU; Initial value; ASTM C518
Maximum Service Temperature, Air 149 °C300 °F
Minimum Service Temperature, Air -183 °C-297 °F
Flammability Test 2525Flame Spread up to 6” (15.23 cm); ASTM E84
 <= 450<= 450Smoke Developed up to 6” (15.23 cm); ASTM E84
 
Descriptive Properties
Closed Cell Content (%)95
ColorYellow
Dimensional Stability (Length Change)plus 0.1%-40°F (-40°C) + Ambient RH/14 days; ASTM D2126
 plus 0.2%212°F (100°C) + Ambient RH/14 days; ASTM D2126
 plus 1.1%158°F (70°C) + 97% RH/14 days; ASTM D2126
Dimensional Stability (Volume Change)minus 0.1%-40°F (-40°C) + Ambient RH/14 days; ASTM D2126
 No Change212°F (100°C) + Ambient RH/14 days; ASTM D2126
 plus 2.3%158°F (70°C) + 97% RH/14 days; ASTM D2126
Hot Surface Performance at 300°F (149°C)PassASTM C411
Polyisocyanurate Insulation RequirementsGrade 2, Type V compliantASTM C591
Water Vapor Transmission2.0 perms/in (2.9 ng/Pa-s-m)ASTM E96

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elliott Company ELFOAM® P200 Polyisocyanurate Foam
Elliott Company ELFOAM® P600 Polyisocyanurate Foam
Elliott Company ELFOAM® P300 Polyisocyanurate Foam
BCC Products MB 1100 Polyurethane Foam Modeling Board
Coastal Enterprises Plus™ PBHT-15 High Density Urethane Foam

PELLIOTT96 / 182685

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.