MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Erbslöh Aluminium DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).

Information provided by PEAK Werkstoff GmbH, a part of Erbslöh Aluminium GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.679 - 2.961 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers >= 144
Tensile Strength >= 123 MPa
@Temperature 300 °C
 >= 338 MPa
@Temperature 200 °C
 >= 491 MPa
@Temperature 20.0 °C
Tensile Strength, Yield >= 122 MPa
@Temperature 300 °C
 >= 318 MPa
@Temperature 200 °C
 >= 429 MPa
@Temperature 20.0 °C
Elongation at Break >= 9.3 %
@Temperature 20.0 °C
 >= 14.4 %
@Temperature 200 °C
 >= 21.2 %
@Temperature 300 °C
Modulus of Elasticity >= 58.0 GPa
@Temperature 300 °C
 >= 65.0 GPa
@Temperature 200 °C
 >= 72.0 GPa
@Temperature 20.0 °C
Poissons Ratio 0.341
@Temperature 20.0 °C
 0.347
@Temperature 100 °C
 0.354
@Temperature 150 °C
 0.361
@Temperature 200 °C
 0.364
@Temperature 250 °C
 0.369
@Temperature 300 °C
Shear Modulus 23.0 GPa
@Temperature 300 °C
 24.0 GPa
@Temperature 200 °C
 24.0 GPa
@Temperature 250 °C
 25.0 GPa
@Temperature 150 °C
 26.0 GPa
@Temperature 100 °C
 28.0 GPa
@Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000570 - 0.00000610 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.9 - 23.9 µm/m-°C
@Temperature 20.0 - 100 °C
 23.7 - 24.7 µm/m-°C
@Temperature 20.0 - 200 °C
 24.5 - 25.5 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 121.9 W/m-K
@Temperature 30.0 °C
 130.9 W/m-K
@Temperature 100 °C
 144.6 W/m-K
@Temperature 200 °C
 155.7 W/m-K
@Temperature 300 °C
 156.1 W/m-K
@Temperature 400 °C
Melting Point 512 - 659 °C
Solidus 512.3 - 518.3 °C
Liquidus 653.6 - 659.3 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 94 %As Balance
Copper, Cu 5.0 %
Titanium, Ti 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Erbslöh Aluminium DISPAL S220 Aluminum Alloy, AlSi35, Condition O
Erbslöh Aluminium DISPAL S270 Aluminum Alloy, AlSi25Fe4Ni3CuMgMnCrTi, Condition T6
Erbslöh Aluminium DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Erbslöh Aluminium DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Erbslöh Aluminium DISPAL S256 Aluminum Alloy, Condition F

NPEAK08b / 170261

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.