MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
TBA ECP 228 Colorable Magnetically Detectable Rotational Molding Powder
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: ECP 228 is based on special blends of magnetic additive compounded into a specially developed easy flow linear polyethylene formulation. The compound is designed to produce moldings of good rigidity combined with excellent impact resistance for use in the food processing industry where magnetic detectability in the food processing line is required. The polymer and flow properties of ECP 228 have been designed to give good moldability over a wide processing window as well as optimizing magnetic properties during molding.

Applications: ECP 228 is recommended for packaging and handling applications where magnetic detection requirements exist.

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.980 g/ccASTM D1505
Melt Flow 6.0 - 9.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ASTM D1706
Tensile Strength, Yield 15.0 - 16.0 MPa50mm/min; ASTM D 638-64T
Elongation at Break 380 - 475 %50mm/min; ASTM D 638-64T
Flexural Modulus 615 MPaASTM D790-66
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 115 °CASTM D1525
Brittleness Temperature -65.0 °CASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTBA010 / 281488

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.