MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polynt HUP 17/18 RN-Ti-grey/34346-PL Sheet Molding Compound Fire Retardancy
Categories: Polymer; Thermoset

Material Notes:

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.74 g/ccPRÜF 09.01
Filler Content 17.9 %PRÜF 10.06A
Water Absorption <= 0.30 %ISO 62
Linear Mold Shrinkage 0.0023 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 125 MPaPRÜF 08.01
Flexural Modulus 8500 MPaPRÜF 08.02
Tensile Impact Strength 45.0 kJ/m²PRÜF 08.03
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 93
Surface Resistance 1.00e+14 ohmIEC 93
Dielectric Strength 20.0 kV/mmIEC 243-1
Comparative Tracking Index 600 VIEC 112
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °CISO 75-2
Flammability, UL94 V-0
@Thickness 4.00 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 135 - 155 °C
Hold Pressure 1160 - 1740 psiMolding pressure
Cure Time 82.5 secPRÜF 10.04
 
Descriptive Properties
Fiber length25 mmPRÜF 03.01
Molding time>25 s/mm
Surface Weight4527 g/m2PRÜF 03.03

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPOLYN9117 / 231712

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.