MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DSM Fibre Intermediates Nyrim® 4000 (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Conditioned at 23°C and 50% Relative Humidity.

Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.

Information provided by the manufacturer, Brueggemann Chemical.

Key Words: RIM materials
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.13 g/ccISO 1183
Moisture Absorption at Equilibrium 1.6 %DIN 53714: 23°C, 50% Relative Humidity
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52ISO 868
Tensile Strength, Ultimate 22.0 MPaISO 527
Elongation at Break 420 %ISO 527
Modulus of Elasticity 0.229 GPaISO 527
Flexural Modulus 0.241 GPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+9 ohm-cmDIN 53482
Surface Resistance 2.00e+8 ohmDIN 53482
Dielectric Constant 4.8
@Frequency 1e+6 Hz
DIN 53483
 15.4
@Frequency 50 Hz
DIN 53483
Dielectric Strength 14.0 kV/mmDIN 53481
Dissipation Factor 0.10
@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 600 VDIN IEC 112 / VDE 030 t1
 
Thermal PropertiesOriginal ValueComments
Melting Point 214 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Brueggemann Chemical Nyrim® 1000 (Dry)
DSM Fibre Intermediates Nyrim® 1500 (Dry)
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin
Brueggemann Chemical Nyrim® 1000 (Conditioned)
CoorsTek Reaction Bonded Silicon Carbide, SCRB (SC-2)

PDSMN080 / 31486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.