MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ DP110 Translucent Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibility

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 30000 - 70000 cPBase
 30000 - 70000 cPAccelerator
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40
Elongation at Break 40 %
Shear Strength 40.0 - 60.0 psiOverlap, Neoprene Rubber/Steel
 80.0 - 100 psiOverlap, SBR/Steel
 150 psiOverlap, Abraded Aluminum, 14 days in 5% salt spray @ 35°C
 250 psiOverlap, Acrylic/Acrylic
 400 psiOverlap, PVC/PVC, Rigid
 500 psiOverlap, ABS/ABS Plastic
 500 psiOverlap. PC/PC
 500 psiOverlap, Etched Aluminum, 14 days in 5% salt spray @ 35°C
 700 psiOverlap, Abraded Aluminum, 3 days, 71°C, 100% RH
 1000 psiOverlap, Al/Al
 1000 psiOverlap, Abraded Aluminum, Initial
 1200 psiOverlap, Etched Aluminum, 3 days, 71°C, 100% RH
 1250 psiOverlap, Abraded Aluminum, 30 days tap water @ RT
 1400 psiOverlap, Fiber Reinforced Polyester/Fiber Reinforced Polyester
 1500 psiOverlap, CRS/CRS
 1500 psiOverlap, Stainless Steel/Stainless Steel
 1500 psiOverlap, Galvanized Steel/Galvanized Steel
 1500 psiOverlap, Copper/Copper
 1500 psiOverlap, Brass/Brash
 2300 psiOverlap, Etched Aluminum, 30 days tap water @ RT
 2500 psiOverlap, Etched Aluminum, Initial
 200 psi
@Temperature 82.0 °C
Overlap
 270 psi
@Temperature 71.0 °C
Overlap
 2500 psi
@Temperature -55.0 °C
Overlap
 2500 psi
@Temperature 24.0 °C
Overlap
Peel Strength 20.0 pliT-Peel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.50e+10 ohm-cm
Dielectric Strength 520 kV/in
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature -50.0 - 0.000 °C
 200 µm/m-°C
@Temperature -50.0 - 110 °C
Thermal Conductivity 1.27 BTU-in/hr-ft²-°F
@Temperature 45.0 °C
Glass Transition Temp, Tg 13.0 °C
 
Descriptive Properties
AppearanceLight YellowAccelerator
 Translucent WhiteBase
 Yellow Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive

PMM34619 / 169366

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.