MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Constellium Alumold® 350 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is particularly suitable for plastic forming machinery operating at temperatures up to 200°C, which is the temperature for molding of rubber and other elastomers.

Information provided by manufacturer

Key Words: IS 5648
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.84 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 110
@Thickness 254 - 305 mm
 120
@Thickness 203.2 - 254 mm
 125
@Thickness 152.4 - 203.2 mm
 135
@Thickness 127 - 152.4 mm
 140
@Thickness 101.6 - 127 mm
 145
@Thickness 7.90 - 50.8 mm
 145
@Thickness 50.8 - 76.2 mm
 145
@Thickness 76.2 - 101.6 mm
Tensile Strength >= 320 MPa
@Thickness 254 - 305 mm
Tempers T851/T852)
 >= 355 MPa
@Thickness 203.2 - 254 mm
Tempers T851/T852)
 360 MPa
@Thickness 254 - 305 mm
Typical Strength
 >= 380 MPa
@Thickness 152.4 - 203.2 mm
Tempers T851/T852)
 390 MPa
@Thickness 203.2 - 254 mm
Typical Strength
 >= 393 MPa
@Thickness 127 - 152.4 mm
Tempers T851/T852)
 >= 407 MPa
@Thickness 101.6 - 127 mm
Tempers T851/T852)
 >= 414 MPa
@Thickness 76.2 - 101.6 mm
Tempers T851/T852)
 420 MPa
@Thickness 152.4 - 203.2 mm
Typical Strength
 >= 428 MPa
@Thickness 7.90 - 50.8 mm
Tempers T851/T852)
 >= 428 MPa
@Thickness 50.8 - 76.2 mm
Tempers T851/T852)
 455 MPa
@Thickness 127 - 152.4 mm
Typical Strength
 465 MPa
@Thickness 7.90 - 50.8 mm
Typical Strength
 465 MPa
@Thickness 50.8 - 76.2 mm
Typical Strength
 465 MPa
@Thickness 76.2 - 101.6 mm
Typical Strength
 480 MPa
@Thickness 101.6 - 127 mm
Typical Strength
Tensile Strength, Yield >= 240 MPa
@Strain 0.2 %,
Thickness 254 - 305 mm
Tempers T851/T852
 >= 270 MPa
@Strain 0.2 %,
Thickness 203.2 - 254 mm
Tempers T851/T852
 >= 280 MPa
@Strain 0.2 %,
Thickness 152.4 - 203.2 mm
Tempers T851/T852
 >= 290 MPa
@Strain 0.2 %,
Thickness 127 - 152.4 mm
Tempers T851/T852
 >= 297 MPa
@Strain 0.2 %,
Thickness 101.6 - 127 mm
Tempers T851/T852
 >= 304 MPa
@Strain 0.2 %,
Thickness 76.2 - 101.6 mm
Tempers T851/T852
 >= 310 MPa
@Strain 0.2 %,
Thickness 50.8 - 76.2 mm
Tempers T851/T852
 310 MPa
@Strain 0.2 %,
Thickness 254 - 305 mm
Typical Strength
 315 MPa
@Strain 0.2 %,
Thickness 203.2 - 254 mm
Typical Strength
 >= 317 MPa
@Strain 0.2 %,
Thickness 7.90 - 50.8 mm
Tempers T851/T852
 330 MPa
@Strain 0.2 %,
Thickness 152.4 - 203.2 mm
Typical Strength
 360 MPa
@Strain 0.2 %,
Thickness 127 - 152.4 mm
Typical Strength
 365 MPa
@Strain 0.2 %,
Thickness 101.6 - 127 mm
Typical Strength
 366 MPa
@Strain 0.2 %,
Thickness 7.90 - 50.8 mm
Typical Strength
 366 MPa
@Strain 0.2 %,
Thickness 50.8 - 76.2 mm
Typical Strength
 366 MPa
@Strain 0.2 %,
Thickness 76.2 - 101.6 mm
Typical Strength
Elongation at Break >= 0.50 %
@Thickness 254 - 305 mm
Tempers T851/T852)
 >= 1.0 %
@Thickness 203.2 - 254 mm
Tempers T851/T852)
 >= 2.0 %
@Thickness 152.4 - 203.2 mm
Tempers T851/T852)
 2.0 %
@Thickness 254 - 305 mm
Typical Elongation
 3.0 %
@Thickness 203.2 - 254 mm
Typical Elongation
 4.0 %
@Thickness 152.4 - 203.2 mm
Typical Elongation
 >= 4.0 %
@Thickness 127 - 152.4 mm
Tempers T851/T852)
 >= 5.0 %
@Thickness 76.2 - 101.6 mm
Tempers T851/T852)
 >= 5.0 %
@Thickness 101.6 - 127 mm
Tempers T851/T852)
 6.0 %
@Thickness 127 - 152.4 mm
Typical Elongation
 >= 6.0 %
@Thickness 50.8 - 76.2 mm
Tempers T851/T852)
 >= 7.0 %
@Thickness 7.90 - 50.8 mm
Tempers T851/T852)
 7.0 %
@Thickness 101.6 - 127 mm
Typical Elongation
 8.0 %
@Thickness 76.2 - 101.6 mm
Typical Elongation
 9.0 %
@Thickness 7.90 - 50.8 mm
Typical Elongation
 9.0 %
@Thickness 50.8 - 76.2 mm
Typical Elongation
Modulus of Elasticity 72.4 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000550 ohm-cmTemper T851
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.3 µm/m-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 130 W/m-KTemper T851

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Composition Spec for Aluminum 305.0
Constellium Alumold® 400 Aluminum
MetalTek Nitronic® 33 Austenitic Stainless Steel
Aluminum 6013-T651
Aluminum 5456-H116; 5456-H321

NCONS012 / 160275

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.