Poly Alloy XuanWu™ XW5101 ABS/PA
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
;
Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
Material Notes:
XuanWu XW5101 resin is an ABS/PA compound with very high impact strength. With high melt flow rate, XW5101 is easy to be processed and performs excellent surface appearance.
Information provided by Poly Alloy Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
1.05
g/cc
1.05
g/cc
ASTM D792
Melt Flow
20
g/10 min
@Load 10.0 kg,
Temperature 240 °C
20
g/10 min
@Load 22.0 lb,
Temperature 464 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength
47.1
MPa
6830
psi
ASTM D638
Elongation at Break
30 %
30 %
ASTM D638
Flexural Strength
58.8
MPa
8530
psi
ASTM D790
Flexural Modulus
1.86
GPa
270
ksi
ASTM D790
Izod Impact, Notched
0.539
J/cm
@Temperature -20.0 °C
1.01
ft-lb/in
@Temperature -4.00 °F
ASTM D256
6.86
J/cm
@Temperature 23.0 °C
12.9
ft-lb/in
@Temperature 73.4 °F
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
90.0
°C
194
°F
ASTM D648
Processing Properties
Metric
English
Comments
Rear Barrel Temperature
220
-
240
°C
428
-
464
°F
Middle Barrel Temperature
230
-
250
°C
446
-
482
°F
Front Barrel Temperature
230
-
250
°C
446
-
482
°F
Nozzle Temperature
230
-
250
°C
446
-
482
°F
Mold Temperature
40.0
-
50.0
°C
104
-
122
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
hour
2.00
hour
Shelf Life
24.0
Month
24.0
Month
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PPALLOY087 / 278366
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.