Key Features:- One component, no mix system
- Fast setting, rapid fixture time
- Bonds well to many substrates
- Less likely to cause “frosting” on substrates
Product Description: Master Bond MB350 is a single component, low viscosity alkoxyethyl cyanoacrylate type system. Unlike most standard cyanoacrylates, MB350 is specially formulated to lessen the possibility of the material leaving a white residue on various substrates. That residue, which appears as a white powdery material, is referred to as blooming or frosting. During the curing process, monomers are released into the air and react with humidity causing a white, powdery material to form. Invariably, it falls back onto the substrate. Many people refer to this as blooming or frosting. This low odor, low bloom system greatly decreases the possibility of this taking place. MB350 is a high strength, rapid curing cyanoacrylate type system. It is a relatively lower viscosity, faster setting system. Similar to other types of “super glue”, MB350 cures very rapidly with the rate of cure dependent upon the humidity—the higher it is, the faster the cure. Because curing is normally fast, minimal contact pressure is usually sufficient for bonding. It must be emphasized that this highstrength system requires no heating or mixing. It typically sets up within 10-40 seconds depending upon the humidity and the substrates. The bond strength is exceptionally high in the shear mode. MB350 bonds well to a variety of substrates, especially to plastics, rubbers and metals. It has reasonably good chemical resistance, especially to cleaning agents. (See chemical resistance table.) The service temperature range for this system is -60°F to +250°F. MB350 is a versatile, high performance cyanoacrylate that can be used in a wide array of different applications in the aerospace, electronic, OEM, electrical, optical and R&D industries. Product Advantages: - Rapid curing at room temperature; usually sets up within 1 minute
- No heating or mixing
- Contact pressure usually sufficient for fixturing
- Bonds well to a wide variety of substrates
- Low odor, low bloom
Information provided by Master Bond Inc. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |