Hostacom XBR 169 G G82299 is a 16% talc filled PP copolymer, with good processability, and surface appearance and scratch resistance and excellent impact/stiffness balance. Low density contributes to reduction of final part weight. The product is available as a customized color matched, pellet form. This grade is delivered in G82299 color version. Applications: Instrument PanelsInformation provided by LyondellBasell. |