MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tropical Dark Red Meranti Wood
Categories: Wood and Natural Products; Wood; Hardwood

Material Notes: Data is based on small, clear, air-dried samples unless specified.
Usual surface texture: Medium
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Variable, generally Moderately Durable (10 to 15 years) to durable
Resistance to penetration by preservatives: Resistant to extremely resistant
Common Applications: Interior and exterior joinery. Plywood

Key Words: Shorea spp.; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.460 g/ccGreen, Asian Origin
Density 0.670 g/ccAir Dry (12-15% Moisture Content)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Wood Indentation 3100 NSide Hardness, Green, Asian Origin
 3500 NSide Hardness, 12% Moisture, Asian Origin
Modulus of Rupture 0.0648 GPaStatic Bending, Green, Asian Origin
 0.0876 GPaStatic Bending, 12% Moisture, Asian Origin
 0.0900 GPaStatic Bending
Flexural Modulus 11.66 GPaStatic Bending
 10300 MPaStatic Bending, Green, Asian Origin
 12200 MPaStatic Bending, 12% Moisture, Asian Origin
Compressive Strength 32.5 MPaParallel to Grain, Green, Asian Origin
 50.7 MPaParallel to Grain, 12% Moisture, Asian Origin
 52.0 MPa
Machinability 50 %Medium Relative to Other Wood
Shear Strength 7.70 MPaParallel to Grain, Green, Asian Origin
 10.0 MPaParallel to Grain, 12% Moisture, Asian Origin
Work to Maximum Load 0.0430 J/cm³Static Bending, Green, Asian Origin
 0.0590 J/cm³Static Bending, 12% Moisture, Asian Origin
 
Thermal PropertiesOriginal ValueComments
Shrinkage 4.5 %Radial; Green to Zero Moisture
 8.2 %Tangential; Green to Zero Moisture
 
Descriptive Properties
ColorMedium to dark red-brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
American Coast Douglas Fir Wood
Pacific Silver Fir Wood
Tropical Light Red Meranti Wood
Tropical American Lemonwood Wood
Tropical Balsa Wood

PTST200 / 71402

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.