MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
NuSil CV1-2960 Silicone, Thermally Conductive
Categories: Polymer; Thermoset; Silicone

Material Notes: General Purpose: Two Part Adhesive and Sealant

Cure system: Platinum

Information provided by NuSil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/cc
Viscosity 900000 cPA
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75
Tensile Strength at Break 1.38 MPa
Elongation at Break 60 %
Tear Strength 55.0 pli
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 1.11 W/m-KASTM E1530
 
Processing PropertiesOriginal ValueComments
Cure Time 4.00 hour
@Temperature 65.0 °C
Tack-Free Time 4.00 hour
Working Life 2.00 hour
 
Descriptive Properties
ColorWhite
Mix Ratio10:1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
NuSil CV-2960 Silicone, Thermally Conductive
NuSil CV1-2964 Silicone, Thermally Conductive
NuSil CV-2948 Silicone, Thermally Conductive
NuSil CV-2946 Silicone, Thermally Conductive
NuSil R-2930 Silicone, Thermally Conductive

PNUSIL193 / 141917

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.